DMP30 > CDI > 2PhI. DSC test results showed that by increasing the amount of accelerator the heat of reaction increased, curing profile became sharp and glass transition temperature remarkably decreased. The broadest curing profile of 14°C also was seen for CDI. The DSC results showed that the reactivity of different accelerators was in order: 2MI > CDI > DMP30 > 2PhI. In other words, 2PhI showed the lowest activity and the sharpest curing profile and 2MI showed the highest activity with the wide curing behavior. It seems that the CDI accelerator at 0.6 phr content would be the best accelerator regarding the highest pot-life at room temperature, high curing rate and maximum Tg.]]>